Product Details:
|
Material: | UNS N02212, Nickel Based Alloys | ||
---|---|---|---|
Highlight: | nickel iron cobalt alloy,high performance alloys,Nickel 212 Special Alloys |
Nickel 212, UNS N02212 W.Nr. 2.4110 sheet, strip, wire, bar, tube etc for electronic parts
1 PRODUCT
Nickel 212, UNS N02212 W.Nr. 2.4110 semi-products for electronic parts.
Nickel 212 is available as sheet, strip, wire, bar, tube etc.
2 EQUIVALENT DESIGNATION
UNS N02212, W.Nr. 2.4110
3 APPLICATION
Nickel 212 has been used in various electronic applications such as electrical lead wires, supporting components in lamps and cathode-ray tube, lamp and electronic valve support assemblies, electrodes in glow-discharge lamps, and ignition contacts etc.
4 OVERVIEW
Nickel
Commercially pure or low-alloy nickel has characteristics that are useful in several fields, notably chemical processing and electronics. Nickel is highly resistant to various reducing chemicals and is unexcelled in resistance to caustic alkalies. Compared with nickel alloys, commercially pure nickel has high electrical and thermal conductivity. It also has a high Curie temperature and good magnetostrictive properties. Annealed nickel has a low hardness and good ductility and malleability. Those attributes, combined with good weldability, make the metal highly fabricable. Nickel has a relatively low work-hardening rate, but it can be cold worked to moderately high strength levels while maintaining ductility.
Nickel 212
Nickel 212 is available as sheet, strip, tube, wire (round, flat, shaped etc), bar etc.
5 CHEMICAL COMPOSITION
Table 1 (wt%)
Ni+Co | C | Cu | Fe | Mg | Mn | S | Si | Co |
≥97.0 | ≤0.10 | ≤0.20 | ≤0.25 | ≤0.20 | 1.5-2.5 | ≤0.006 | ≤0.20 | ≤1.0 |
6 PHYSICAL PROPERTIES
Density: 8.86 g/cm3 (0.320 lb/in3)
Melting range: 1435-1446°C (2615-2635°F)
Specific heat: 430 J/kg•°C (0.103 Btu/lb•°F)
Coefficient of Expansion : (68-212°F / 20-100°C): 7.2x10-6 in/in•°F (12.9um/m•°C)
Thermal Conductivity: 305 Btu•in/ft2•h•°F (44.0W/m•°C)
Electrical Resistivity: 66 ohm•circ mil/ft (0.109uohm•m)
Shear modulus: 78 kN/mm²(11313 ksi)
Elasticity modulus: 196 kN/mm²(28400 ksi)
7 MECHANICAL PROPERTIES
Thanks to the addition of manganese, the strength is stronger than Nickel 200.
Tensile strength and elongation at temperatures above 315°C (600°F) dropped significantly.
Working temperature is related to environment, load and size range.
Condition | Approximate tensile strength | |
MPa | ksi | |
Annealed | 450-550 | 65-80 |
Cold drawn hard | 750-950 | 109-138 |
Norminal mechanical properties as per DIN 17750 (Plate, strip and sheet)
Code | W.Nr.No. | Condition | Heat treatment | Strip thickness mm | Plate thickness mm | Rm N/mm2 min. | Rp0.2 N/mm2 min. | Rp1.0 N/mm2 min. | Elongation A5 % min. | Brinel Hardness HBW 2.5/62.5 | |
max. | about | ||||||||||
NiMn2 | 2.4110 | F40 | Annealed | 0.20-2.50 | / | 400 | 140 | / | 40 | 130 | / |
F54 | Half hard | 0.20-2.50 | / | 540 | 340 | / | 20 | / | 160 | ||
F74 | Hard | 0.20-2.50 | / | 740 | 600 | / | 2 | / | 220 |
Norminal mechanical properties as per DIN 17753 (Wire)
Code | W.Nr.No. | Condition | Heat treatment | Dia.mm | Rm N/mm2 min. | Elongation | |
AL=100 % min. | A5 % min. | ||||||
NiMn2 | 2.4110 | F40 | Annealed | 0.10≤d≤0.30 | 400 | 15 | / |
F40 | Annealed | 0.30<d≤0.80 | 400 | 20 | / | ||
F40 | Annealed | 0.80<d≤3.00 | 400 | 30 | / | ||
F40 | Annealed | 3.00<d≤8.00 | 400 | / | 30 |
8 STANDARD SPECIFICATION
DIN 17741 Low-alloy wrought nickel alloys - Chemical composition
DIN 17750 Plates, strips and sheets of wrought nickel and nickel alloys - properties
DIN 17751 Tubes of wrought nickel and nickel alloys - Properties
DIN 17752 Rod and bar of wrought nickel and nickel alloys - Properties
DIN 17753 Wires of wrought nickel and nickel alloys - Properties
9 COMPETITIVE ADVANTAGE:
(1) More than 50 years experience of research and develop in high temperature alloy, corrosion resistance alloy, precision alloy, refractory alloy, rare metal and precious metal material and products.
(2) 6 state key laboratories and calibration center.
(3) Patented technologies.
(4) Ultra-purity smelting process: VIM + IG-ESR + VAR
(5) Excellent high performance.
10 BUSINESS TERM
Minimum Order Quantity | Negotiable |
Price | Negotiable |
Packaging Details | Water prevent, seaworthy transport, mill’s export standard packing |
Mark | As per order |
Delivery Time | 60-90 days |
Payment Terms | T/T, L/C at sight, D/P |
Supply Ability | 100 metric tons / Month |
Contact Person: Mr. lian
Tel: 86-13913685671
Fax: 86-510-86181887